MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SACO AEI PEXIDAN® L/T-Flex Moisture-curable PE compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: PEXIDAN® L/T Flex is a medium density PEX system consisting of a silane grafted base-compound A- 1025 and a catalyst masterbatch CAT-003 and featuring much improved flexibility over high density PEX pipe materials. When mixed and extruded in the proper proportions, the two-component system results in a material that is crosslinkable by exposure to moisture or by immersion in hot water at 90-95°C. PEXIDAN® L/T Flex meets NSF International Standard 14 and ASTM F876 standard for non-potable water pressure pipe applications. The system is available in red, white, blue and natural, or can be colored at extrusion.

Information provided by SACO AEI Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.939 g/ccASTM D792
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature <= 30.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3700 psiASTM D638
Tensile Strength, Yield 2900 psiASTM D638
Elongation at Break 250 %ASTM D638
Flexural Modulus 80000 psi2% secant; ASTM D790
Tensile Set 0.00 %
@Treatment Temp. 150 °C,
Time 900 sec
Permanent elongation after cooling after 23% elongation under load, 20N/cm2; SACO AEI DWI-QA-4007 based on ICEA T-28-562
 
Processing PropertiesOriginal ValueComments
Processing Temperature 320 - 350 °Fbarrel
Head Temperature 365 °F
 365 °F
 
Descriptive Properties
Degree of Crosslinking>80%ASTM D2765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO072 / 265502

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.