MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker ELASTOSIL® LR 3003/82 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Liquid silicone rubbers of the ELASTOSIL® LR 3003 series are paste-like, easily-pigmentable two-component compounds with short curing times. Their vulcanizates are noted for their high transparency and excellent mechanical and electrical properties.

Properties: Narrow Shore hardness range from 78 to 84. The products can be used within a temperature range of - 55 °C to + 210 °C. The addition of heat stabilizers at service temperatures of more than 180 °C is recommended.

Application: These grades are particularly suitable for the economical production of large series of injection-molded articles. Parts made from ELASTOSIL® LR 3003/82 A/B can be used for technical applications. These articles are also suitable for use in conjunction with foodstuffs. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccISO 1183-1 A
Viscosity 480000 cP
@Shear Rate 10.0 1/s
DIN EN ISO 3219
 1.30e+6 cP
@Shear Rate 1.00 1/s
DIN EN ISO 3219
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82DIN 53505
Tensile Strength 1015 psiISO 37
Elongation at Break 140 %ISO 37
Compression Set 16 %
@Temperature 175 °C,
Time 79200 sec
DIN ISO 815-B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °Cheat stabilizers recommended > 180°C
Minimum Service Temperature, Air -55.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Transparent, but not quantified
 
Descriptive Properties
AppearanceTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker ELASTOSIL® LR 3003/90 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3003/30 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3003/25 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3003/20 TR A/B Liquid Silicone Rubber
Dow Silastic® 9280/60E KIT PARTS A&B

PWACK9924 / 197523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.