MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics CVD Silicon Carbide
Categories: Ceramic; Carbide

Material Notes: 99.9995% ultra-pure Chemically Vapor Deposited (CVD) silicon carbide with unique microstructure. Offers outstanding thermal properties and superior chemical and erosion resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.21 g/ccFired
Porosity 0.00 %Apparent, fully dense
Particle Size 2.0 - 10 µmGrain size
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 28000MPa, at Hv 0.5kg
Modulus of Elasticity 450 GPa
@Temperature 20.0 °C
Flexural Strength 450 MPa
@Temperature 20.0 °C
4-point
Fracture Toughness 3.00 MPa-m½
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.010 - 10000 ohm-cm
@Temperature 20.0 °C
Van der Pauw
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µm/m-°C
@Temperature 20.0 - 950 °C
Thermal Conductivity 250 W/m-K
@Temperature 20.0 °C
 
Descriptive Properties
Thermal Downshock660Change in °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoorsTek UltraSiC™ SC-30 Direct Sintered Silicon Carbide
CeramTec CD 110 Silicon Carbide, SSiC
CeramTec Rocar® ST Silicon Carbide, SSiC
CoorsTek Pure SiC™ LR CVD Silicon Carbide, > 99.9995%
CeramTec Rocar® S Silicon Carbide, SSiC

CMORG59 / 90437

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.