MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen RP348R Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Moplen RP348R is a polypropylene random copolymer with good flowability which is used in injection molding applications. Moplen RP348R is nucleated, for improved productivity and very good optical properties (transparency and brilliance). Its antistatic activation prevents dust deposits and eases items demolding. Typical applications of Moplen RP348R are caps & closures, house wares and rigid packaging items. Applications: Caps & Closures, House wares.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 25 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 29.0 MPaASTM D638
Elongation at Yield 13 %ASTM D638
Flexural Modulus 1050 MPaASTM D790
Izod Impact, Notched 45.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CASTM D648
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Moplen RP348N Polypropylene Copolymer
LyondellBasell Moplen RP2380 Polypropylene Copolymer
LyondellBasell Moplen RP2965 Polypropylene Copolymer
LyondellBasell Moplen RP344NK Polypropylene Copolymer
LyondellBasell Moplen RP346R Polypropylene Copolymer

PEQT9107 / 220738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.