MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Metflex M11 NBR 50; Acrylonitrile butadiene rubber with low-medium CAN content
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Oil resistant rubber for use at relatively low temperatures. Good adhesion to steel. Normally used in seals, o-rings and hoses, specially compounded by Metflex for gas diaphragms. Meets the requirements of EN 13787.

Information provided by Metflex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 13.2 MPaISO 37: Type 2
 13.86 MPa
@Treatment Temp. 100 °C,
Time 605000 sec
Heat Age; ISO 188
Elongation at Break 383 %ISO 37: Type 2
 325.55 %
@Treatment Temp. 100 °C,
Time 605000 sec
Heat Age; ISO 188
Compression Set 15 %
@Temperature 100 °C,
Time 86400 sec
ISO 815
 32 %
@Temperature -20.0 °C,
Time 259000 sec
ISO 815
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °C
Minimum Service Temperature, Air -20.0 °C
 
Descriptive Properties
International Rubber Hardness Degrees60.146IRM 902 168 hr at 100°C, ISO 1817
 61ISO 48
 64.66Heat Age, 168hrs at 100°C, ISO 815
Static OzonePass
Weight Change0.01IRM 902 168 hr at 100°C, ISO 1817
 0.05n-PENTANE 72 hrs at 23°C (wet), ISO 1817
 -0.05n-PENTANE 72 hrs at 23°C (dried 168 hrs at 40°C), ISO 1817

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Metflex M108 NBR 50; Acrylonitrile butadiene rubber with low-medium CAN content
Metflex M52 NBR 50; Acrylonitrile butadiene rubber with low-medium CAN content
EMS-Grivory Grilamid® L 20 EC PA12-CD25
Avient PolyOne® ND-10 Ethylene-Propylene Diene Elastomer (EPDM) Compound

PMETF003 / 190818

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.