MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Engage® 8402 Polyolefin Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: Engage® 8402 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8402 provides high clarity in products requiring visual inspection and allows the use of hot runner molds to enhance production efficiency. In addition, its low density can help control resin and production costs, while reducing the weight of end products.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccASTM D792
Melt Index of Compound 30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94ASTM D2240
Hardness, Shore D 44ASTM D2240
Tensile Strength, Ultimate 12.9 MPa508 mm/min; ASTM D638
Tensile Strength, Yield 6.30 MPa508 mm/min; ASTM D638
Elongation at Break 790 %508 mm/min; ASTM D638
2% Secant Modulus 0.0699 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 98.0 °CDSC, 10°C/min; DuPont Test
Vicat Softening Point 76.0 °CASTM D1525
 
Descriptive Properties
Comonomer Content22 wt%Dow Method (13C NMR/FTIR)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Engage® 8407 Polyolefin Elastomer
Dow Engage® 8401 Polyolefin Elastomer
Dow Engage® 8440 Polyolefin Elastomer
Dow Engage® 8842 Polyolefin Elastomer
Dow Engage® 8200 Polyolefin Elastomer

PDVE37 / 34098

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.