MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
E-Polymers SEPAZ® K130IM 30% Glass Fiber Reinforced Impact Modified PPS Resin
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler

Material Notes: Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidity leads to good dimensional precision. SEPAZ PPS applications: switches, connectors and other electronic and electric components, alternators and other automobile components, and office equipment components including chassis parts and housings.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Water Absorption 0.020 %
@Time 86400 sec
Linear Mold Shrinkage 0.0030 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 142.2 MPaASTM D638
Elongation at Break 4.0 %ASTM D638
Flexural Strength 235.44 MPaASTM D790
Flexural Modulus 9025.2 MPaASTM D790
Izod Impact, Notched 14.0 kg-cm/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.8
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 245 °CASTM D648
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Melt Temperature 300 - 330 °C
Mold Temperature 130 - 160 °C
Drying Temperature 140 °C
Dry Time 6 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® SF-40GF-10 MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
Avient Edgetek® SF-35GF-25MN/000 L Polyphenylene Sulfide (PPS), Glass/Mineral Filled
Celanese FORTRON 1131L4 ITT PPS, 30% Glass Reinforced
Celanese Fortron® 1130 L4 Polyphenylene Sulfide (PPS), 30% Glass Fiber
Avient Edgetek® SF-35GF-15MC/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled

PEPOLZ058 / 103555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.