MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotchlite™ S60/10000 Glass Bubbles
Categories: Ceramic; Glass; Other Engineering Material; Additive/Filler for Polymer

Material Notes: High-strength polymer additives made from a water-resistant and chemically-stable soda-lime-borosilicate glass. These hollow glass microspheres can be used as a low density filler material ideal for plastic and rubber parts created from injection molding, extrusion processes and/or other vigorous processing equipment (Banbury mixers, etc.). Scotchlite glass bubbles help to reduce weight; reduce thermal expansion; and contribute to cost savings. They are used as additive materials in the automotive, truck, rail and aerospace industries.

Information supplied by 3M Specialty Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.600 g/ccTrue Density
Bulk Factor 0.63Packing factor (bulk density to true particle density)
Oil Absorption 33.5 %g oil/100 cc of polymer additive
Loss On Ignition <= 0.50 %Volatile content (by weight)
Particle Size 30 µmAverage diameter
pH 9.5at 5% loading in water
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 10000 psiIsostatic crush strength
 
Thermal PropertiesOriginal ValueComments
Softening Point 600 °C
 
Descriptive Properties
Alkalinity0.5 milliequivalents/gram max.
Color, Unaided EyeWhite, powdery
CompositionSoda-lime-borosilicate glass
Flotation92% by volumedensity<1.0 g/cc
ShapeHollow glass spheres with thin walls

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M K11 Glass Bubbles
3M K42HS Glass Bubbles
Nickel, Ni
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler
301 Stainless Steel

CMMMS01 / 1619

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.