MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Geon® Performance Solutions 210 Series 215 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Geon® 215 is a low molecular weight particle size homopolymer blending resin intended for use in plastisol formulations. It improves air release performance resulting in reduced scrap rates. It decreases high shear viscosity providing an improved 'ease of coating' performance resulting in a more uniform plastisol coating and improving line up time. It reduces viscosity aging characteristics, providing increased plastisol usage (pot life). It reduces surface gloss of films or coated products resulting in less surface blocking and improved handling. Geon® 215 is recommended for solid and foamed plastisol applications such as coated fabric, cast films and coatings, foam mats and pads.

Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC (formulation): 60phr Geon® 121A, 40phr Geon® 215, 57phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 1203(formulation): 60phr Geon® 178, 40phr Geon® 215,and 60phr DOP

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Volatiles 0.060 %0.060 %Geon® STP 1242; Internal Method
Apparent Bulk Density 0.430 g/cc0.0155 lb/in³Geon® STP 1169; Internal Method
Particle Size 25 µm25 µmGeon® DFT 1466; Internal Method
 <= 52 µm<= 52 µm98%; Geon® DFT 1466; Internal Method
 <= 74 µm<= 74 µm99.8%; Geon® DFT 1466; Internal Method
Relative Viscosity 2.12 cP2.12 cPCorrelation, Cyclohexanone 1%; Internal Method
Brookfield Viscosity 3.4 cP3.4 cPInitial Viscosity @ 2rpm Geon® ALTC 22 (with provided formulation); Internal Method
 3.5 cP3.5 cPInitial Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
 4.0 cP4.0 cPOne Day Viscosity @ 2rpm Geon® ALTC 22 (with provided formulation); Internal Method
 4.23 cP4.23 cPOne Day Viscosity @ 20rpm Geon® ALTC 22 (with provided formulation); Internal Method
Viscosity Measurement 0.850.85Inherent; ASTM D1243-60-A
Melt Flow 276 g/10 min
@Pressure 0.655 MPa
276 g/10 min
@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
 
Optical PropertiesMetricEnglishComments
Haze 20 %
@Temperature 177 °C
20 %
@Temperature 351 °F
Fused 5 mins Geon® ALTC 66 (with provided formulation); Internal Method
Gloss 20 %
@Temperature 177 °C
20 %
@Temperature 351 °F
60° Fused 5 mins Geon® ALTC 65 (with provided formulation); Internal Method
 
Descriptive Properties
FormsPowder
Gel Temperature78 °CInternal Method; Geon® ALTC 29 (with provided formulation)
Generic MaterialPVC Homopolymer
Generic NamePolyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value64No Standard; Correlation, 0.5g/100ml
Polymerization ProcessSuspension
Processing MethodCasting
 Dip Coating
 Rotational Molding
 Slush Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Residual Vinyl Chloride Monomer< 5 ppmInternal Method; Geon® STP 1005
Vinyl Dispersion Gauge75 µmInternal Method; Geon® STP 1203 (with provided formulation)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 120 Series 129 Polyvinyl Chloride Homopolymer
Geon® Performance Solutions 120 Series 120X400 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions FIT E 50 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Lanxess Mesamoll® II Plastic Additive

PH0POL1431 / 146000

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.