MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMELT® A6453 Polyamide  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product properties: Evonik’s VESTAMELT®iS combines good adhesion to various substrates, good chemical resistance and excellent mechanical properties with high transparency. This offers prospects for new product designs that have been unavailable to date, particularly in the area of LED lighting and sensor products where transparency is a must.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Viscosity 50 cP
@Temperature 200 °C
Melt
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70JIS K7215
Tensile Strength at Break 36.0 MPa
Elongation at Break 400 %
Tensile Modulus 410 MPa
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched NBISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmJIS K6911
Dielectric Constant 3.2
@Frequency 1e+6 Hz
VDE 303
Dielectric Strength 29.0 kV/mmIEC 60243-1
Dissipation Factor 0.049
@Frequency 1e+6 Hz
VDE 303
Comparative Tracking Index >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 140 µin/in-°FISO 11359
Thermal Conductivity 0.300 W/m-K
Melting Point 170 °CISO 1346
Maximum Service Temperature, Air 100 °C
Vicat Softening Point 131 °CISO 306
Minimum Service Temperature, Air -30.0 °C
Glass Transition Temp, Tg 20.0 °C
Flammability, UL94 V-2
@Thickness 1.60 mm
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.52JIS K7215
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 220 °C
Nozzle Temperature 200 - 230 °C
Zone 1 130 - 140 °C
Zone 2 150 - 160 °C
Zone 3 180 - 200 °C
Mold Temperature >= 20.0 °C
Drying Temperature 70.0 °C
Dry Time 4.00 hour
 
Descriptive Properties
Colortransparent or black
Funnel20-30°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Trogamid® CX7323 Transparent Nylon
Evonik Trogamid® A4000 Transparent Polyamide
Lotte Advanced Materials Infino® TP-1020 PC, Unreinforced Transparent
EMS-Grivory Grivory® G 16 PA6I/6T
EMS-Grivory Grilamid® TR 30 LS nat PA*

PEVONIL230 / 196434

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.