MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Composition Spec for Aluminum 243.0
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: The sum of 'Other' metallic elements 0.010 percent or more each, expressed to the second decimal before determining the sum.

The aluminum content for unalloyed aluminum not made by a refining process is the difference between 100.00 percent and the sum of all other metallic elements present in amounts of 0.010 percent or more each, expressed to the second decimal before determining the sum.

Includes listed elements for which no specific limit is shown.

This database entry lists the complete composition spec as collected by TheMetalMarket. Other database entries have complete physical property data for most aluminum alloys.

Key Words: UNS A02430 (Obsolete); Aluminium 243.0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 88.7 - 92.33 %
Chromium, Cr 0.20 - 0.40 %
Copper, Cu 3.5 - 4.5 %
Iron, Fe <= 0.40 %
Magnesium, Mg 1.8 - 2.3 %
Manganese, Mn 0.15 - 0.45 %
Nickel, Ni 1.9 - 2.3 %
Other, each <= 0.050 %
Other, total <= 0.15 %
Silicon, Si <= 0.35 %
Titanium, Ti 0.060 - 0.20 %
Vanadium, V 0.060 - 0.20 %
Zinc, Zn <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6025 Composition Spec
Aluminum 3103B Composition Spec
Aluminum 2618-T6
Aluminum 242.0-T61, Sand Cast
7024 Aluminum Composition Spec

MX2031 / 14335

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.