MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Mineral Colloid® MO Clay Additive
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Mineral Colloid MO is a high purity, highly thixotropic beneficiated montmorillonite. Because of its thixotropic nature, Mineral Colloid MO gives excellent sag control, leveling properties, and syneresis control to water borne paint systems. Mineral Colloid MO is easy to disperse and can be used over a wide pH range.

Applications:

  • Latex Emulsion Paint Systems
  • Water Reducible Alkyds
  • Water Base Stains
  • Water Base Inks

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 9.52% Solids
Brookfield Viscosity 2000 cP3% Solids, 50 rpm
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 8.0 %
 
Descriptive Properties
Color/FormOff white, fine powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Laponite® XLS Synthetic Layered Silicate
BYK Laponite® XLG Synthetic Layered Silicate
BYK Nanothix® B1490 Phylosilicate
BYK Mineral Colloid® BP Bentonite
BYK Laponite® XL21 Synthetic Layered Silicate

PBYK074 / 185071

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.