MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Dexflex 727-UV YGYA Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Dexflex thermoplastic polyolefins (TPOs) are in use in applications once reserved for more expensive engineering resins. The performance of these TPOs, combined with their quality and consistency, makes them cost-effective alternatives in automotive applications.

Dexflex 727-UV YGYA very high melt flow, medium flexural modulus, UV-stabilized, mineral-filled, thermoplastic elastomeric olefin has an excellent balance of properties and processability. Applications: Automotive Parts, Exterior Automotive Applications

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 230 °C
19 g/10 min
@Load 4.76 lb,
Temperature 446 °F
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus, 1% Secant 850 MPa123000 psi
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Spartech Spectrum® S370 TPO Polyolefin Sheet
LyondellBasell Dexflex 815 BLK XXX Thermoplastic Polyolefin
LyondellBasell Dexflex 727-UV 4LLA Thermoplastic Polyolefin
Ensinger TECAPEI® made from Ultem® 1000 PEI
Canuck Compounders BK 8-8-6R Automotive Grade Mineral Filled Black Thermoplastic PolyOlefin (TPO)

PEQT7112 / 218749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.