MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polikim ULPOLEN® 500 UHMWPE Standard
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to special types with additives. One major problem in the identification and selection of materials is the difficulty in distinguishing Ulpolen® 1000 from other lower quality polyethylene types in terms of physical apperance. The main differences in technical properties are evidenced in laboratory tests. Variations of Ulpolen® 1000 within its group according to molecular weights and its physical similarity to other polyethylene types are vital factors that should be carefully studied to select the right material for the application. In addition to “1000” quality, there are subgroups with different technical properties such as Ulpolen® 500 which is primarily used in food industry as cutting plates (with 0.5 million molecular weight) and Ulpolen® 300 which is used in chemical industry in the production of tanks resistant to chemicals (with 0.3 million molecular weight).

Information provided by Polikim Polimer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³DIN 53479
Water Absorption at Saturation 0.00 %0.00 %ASTM D570
Molecular Weight 500000 g/mol500000 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60 - 6860 - 68DIN 53505
Tensile Strength, Ultimate 24.5 MPa3560 psiDIN 53455
Elongation at Break >= 300 %>= 300 %DIN 53455
Izod Impact, Notched (ISO) NBNBDIN 53453
Charpy Impact Unnotched >= 2.50 J/cm²>= 11.9 ft-lb/in²ISO 11542/2
Coefficient of Friction 0.15 - 0.200.15 - 0.20
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.4 kV/mm899 kV/inDIN 53481
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C111 µin/in-°FDIN 53752
Melting Point 130 - 138 °C266 - 280 °FISO 3146
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -100 °C-148 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polikim ULPOLEN® 1000 UHMWPE Standard
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer
Overview of materials for High Density Polyethylene (HDPE), Film Grade
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE
Overview of materials for Low Density Polyethylene (LDPE), Molded

PPOLIK017 / 99827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.