MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ 8600-10 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: EMERGE™ PC 8600-10 is a translucent, ignition-resistant polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global environmental standards. It is an easy flow PC resin suitable for use in injection molded applications in the computer, electronics, electrical, and information technology equipment markets.

Application:

  • Information technology equipment
  • Electronics and electrical appliances
  • Battery chargers and adaptors

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmFlow; ASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 123ASTM D785
Tensile Strength, Ultimate 8400 psi0.125 in, injection molded; ASTM D638
Tensile Strength, Yield 8700 psi2in/min, 0.125 in specimen, injection molded; ASTM D638
Elongation at Break 110 %0.125 in, injection molded; ASTM D638
Elongation at Yield 6.2 %0.125 in, injection molded; ASTM D638
Tensile Modulus 320000 psi0.125 in, injection molded; ASTM D638
Flexural Strength 13600 psi0.125 in, injection molded; ASTM D790
Flexural Modulus 348000 psi0.125 in, injection molded; ASTM D790
Izod Impact, Notched 14.0 ft-lb/in0.125 in, injection molded; ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Thickness 4.00 mm
ISO 180/A
Dart Drop, Total Energy 58.8 J0.125 in, injection molded; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 36.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 282 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °FASTM D648
Vicat Softening Point 144 °CISO 306/B50
 150 °CISO 306/A120
 300 °F120°C/hr, 10N; ASTM D1525
UL RTI, Electrical 257 °FUL 746
UL RTI, Mechanical with Impact 257 °FUL 746
UL RTI, Mechanical without Impact 257 °FUL 746
Flammability, UL94 V-0
@Thickness 1.50 mm
Oxygen Index 35 %ASTM D2863
Glow Wire Test 960 °C
@Thickness 2.00 mm
IEC 695-2-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 271 - 288 °C
Mold Temperature 66.0 - 99.0 °C
Drying Temperature 121 °C
Dry Time 3 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo EMERGE™ 8600-20 Polycarbonate
AK Steel 316 Austenitic Stainless steel
Trinseo CALIBRE™ 5201 15 Polycarbonate, 20% Glass Reinforced
A. Schulman Diamond PC-1212FRO Natural, Flame Retardant Polycarbonate
Alclad Aluminum 6061-T6, T651

PZZDOW1369 / 30587

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.