MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Features: Good Flexibility at Low Temperatures and Improved Weathering Performance.

Uses: Flat Die/Cast Film Extrusion and Hose/Profile Extrusion, Injection Molding.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.014 cm/cmInjection
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82 - 88
@Time 5.00 sec
ASTM D2240
Tensile Strength 48.3 MPaASTM D412
Elongation at Break 550 %ASTM D412
100% Modulus 0.00550 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0104 GPa
@Strain 300 %
ASTM D412
Tear Strength 130 pliTrouser; ASTM D470
Graves Tear Strength 500 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 20H18, 1000g; ASTM D3389 B
Tensile Set 10 %200% elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °CDSC
Glass Transition Temp, Tg -32.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 177 °CInjection
Middle Barrel Temperature 188 °CInjection
Front Barrel Temperature 193 °CInjection
Nozzle Temperature 199 °CInjection
Zone 1 177 °CExtrusion
Zone 2 183 °CExtrusion
Zone 3 188 °CExtrusion
Zone 4 194 °CExtrusion
Adapter Temperature 194 °C5, Extrusion
Die Temperature 194 °CZone 1, 6, Extrusion
 194 °CZone 2, Extrusion
Melt Temperature 155 °CKofler
 199 °CInjection
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
Injection Pressure 3000 - 7000 psiInjection
Back Pressure 50.0 psiInjection
Screw Speed 20 - 50 rpmInjection
 
Descriptive Properties
Volume swell in Jet Fuel JP87.7%ASTM D471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer
Nexeo® HIVAL® 500354 High Density Polyethylene
Envalior Arnitel® EM630-H Polyether Ester Elastomer (European Grade)
Lubrizol Estane® 58070 Thermoplastic Polyurethane

PNOVEON030 / 55296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.