MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Isobutanol
Categories: Fluid; Solvent

Material Notes: Formula: C4H10O

CAS: 78-83-1

Description: Isobutanol is a clear, mobile, neutral liquid with a characteristic odor. It is miscible with all common solvents, e.g., alcohols, ketones, aldehydes, ethers, glycols, and aromatic and aliphatic hydrocarbons, but is only sparingly soluble in water.

Applications: A large part of the isobutanol produced is converted into derivatives(primarily esters) for use as solvents in the coatings industry. Isobutanol is an eminently suitable solvent for acid-curable lacquers and baking finishes derived from urea (Plastopal), melamine (Luwipal), or phenolic resins. When added even in small proportions to alkyd resin paints, isobutanol reduces the viscosity, and thus improves the brushability and flow. Diisobutyl phthalate (DIBP) is an established plasticizer for plastics, dispersions and rubber mixes. Other isobutyl esters of dicarboxylic acids, e.g., adipic, azelaic and sebacic acids, display good properties in this application, but economic considerations preclude their use.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.802 - 0.804 g/cc
Molecular Weight 74.1 g/mol
 
Thermal PropertiesOriginal ValueComments
Distillation Temperature 106 - 108 °C
@Pressure 0.101 MPa
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %ASTM D1364
 
Descriptive Properties
Acidity, as HCI0.0003as acetic acid, ASTM D1613
Assay>99.5%
Color<5ASTM D1209

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF N-Butanol
BASF Dibutylamine
BASF Butylamine
ExxonMobil Santoprene® 181-57W180 Thermoplastic Elastomer
ExxonMobil Santoprene® 121-70B230 Thermoplastic Elastomer

PBASG0983 / 132616

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.