MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature. These electronic grade silicone adhesive sealants differ somewhat in physical properties including consistency.

Key Performance Properties:

  • Non-corrosive to electronic metals, including copper and brass
  • Low odor cure, releasing an alcohol vapor from the sealant surface during cure
  • UL recognition
  • Retains elastomeric properties for long periods at temperatures from 60°C to 205°C and for short periods up to 260°C
  • One-component
  • Cure at room temperature
  • Excellent electrical insulation properties
  • Excellent resistance to moisture, dust, dirt, UV, ozone, and chemicals

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
Viscosity 38000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25
Tensile Strength, Ultimate 19.0 kg(f)/cm²
Elongation at Break 230 %
Peel Strength 10.0 pli1 in. x 8in. Stainless steel screen at 180° pull angle
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+14 ohm-cm
Dielectric Constant 2.8
@Frequency 60 Hz
Dielectric Strength 20.0 kV/mm
Dissipation Factor 0.0010
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 270 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.000500 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 204 °CContinuous
 260 °CIntermittent
Brittleness Temperature -60.0 °C
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 4 hour
 
Descriptive Properties
ColorWhite
ConsistencyFlowable liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray
Momentive Performance Materials RTV162 Electronic Grade Silicone Adhesive Sealant, White
Momentive Performance Materials RTV160 White Adhesive Sealant, Non-Corrosive Pourable

PGESIL023 / 41014

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.