System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Omni Plastics OmniPro™ HPP TF20 CBFR0 Homopolymer Polypropylene, 20% Talc reinforced
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 20% Talc Filler
Material Notes:
20% Talc reinforced, bromine and chlorine free, flame resistant; values are based on natural or black materials unless otherwise noted.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.18
g/cc
ASTM D792
Filler Content
20 %
ASTM D2584
Melt Flow
12
g/10 min
ASTM D1248
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
26.0
MPa
ASTM D638
Elongation at Break
10 %
ASTM D638
Flexural Strength
50.0
MPa
ASTM D790
Flexural Modulus
3585
MPa
ASTM D790
Izod Impact, Notched
32.0
J/m
@Thickness 3.17 mm
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
138
°C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94
V-0
@Thickness 3.00 mm
UL Submission Pending
Processing Properties
Original Value
Comments
Rear Barrel Temperature
400
-
480
°F
Middle Barrel Temperature
420
-
500
°F
Front Barrel Temperature
420
-
500
°F
Nozzle Temperature
420
-
500
°F
Melt Temperature
420
-
500
°F
Mold Temperature
80.0
-
140
°F
Back Pressure
50.0
-
100
psi
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant
Multibase Multi-Flam™ 0206 PP Polypropylene
Multibase Multi-Flam™ 0220 PP Polypropylene
Multibase Multi-Flam™ 0302 PP NH Polypropylene
POMNI5084 / 185230
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.