MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form as well as blended with other PE resins, such as LDPE or HDPE and mPE resins for mono extrusion of co-extrusion process to modify film properties.

Lotrene® Q2018 Series are suited for many applications in the field of consumer, industrial, food or hygiene packaging such as freezer film, bread bags, shoppers and bags as well as lamination film and multilayer packaging film.

Lotrene® Q2018N is a blown film grade and contains thermal stabilizers.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.918 g/cc0.918 g/ccISO 1183
Thickness 40.0 microns1.57 mil
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 0.000 ppm0.000 ppm
Slip Level 0.000 ppm0.000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiASTM D882
Film Elongation at Break, MD 850 %850 %ASTM D882
Film Elongation at Break, TD 900 %900 %ASTM D882
Elmendorf Tear Strength, MD 5.60 g/micron142 g/milASTM D1922
Elmendorf Tear Strength, TD 10.7 g/micron272 g/milASTM D1922
Dart Drop Test 130 g0.287 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 35.0 MPa5080 psiASTM D882
Film Tensile Strength at Break, TD 32.0 MPa4640 psiASTM D882
1% Secant Modulus, MD 215 MPa31200 psiASTM D882
1% Secant Modulus, TD 245 MPa35500 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 121 °C250 °FCrystalline; ISO 11357
Vicat Softening Point 100 °C212 °FASTM D1525 (A120)
 
Optical PropertiesMetricEnglishComments
Haze 14 %14 %ASTM D1003
Gloss 55 %55 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 210 °C338 - 410 °FExtrusion
Melt Temperature 190 °C374 °F
Die Opening >= 0.180 cm>= 0.0709 in
Blow-up Ratio (BUR) 2.0 - 3.02.0 - 3.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film
Braskem LL 218/21 LLDPE Blown Film Extrusion Polyethylene
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film
LyondellBasell Plexar® PX3227 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
LyondellBasell Plexar® PX3216 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE

PTOTAL769 / 130494

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.