MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NaturePlast NPW SEA 230 Biopolyester
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polylactic Acid (PLA) Biopolymer

Material Notes: General Properties: The NPW SEA range consists of a set of Biocomposites which can be produced from oil based as well as biobased or biodegradable polymers. The by-products used here as fillers are waste material from seashell.

Applications:
Process:

  • Primarily injection molding
  • Adaptable to other processes
Markets:
  • Rigid secondary packaging
  • Regular consumption goods
  • Technical parts
  • Agriculture / horticulture
  • Cosmetic / luxury
Properties:
  • Partially to totally biobased
  • Some of them are biodegradable and compostable
  • Rigid
  • Natural appearance

Information provided by NaturePlast Bioplastics Experts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 27 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 7.9 %ISO 527
Tensile Modulus 1690 MPaISO 527
Charpy Impact Unnotched 32.0 kJ/m²ISO 179
 
Descriptive Properties
FillerOyster
Filling Rate0.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNATPLAS055 / 285504

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.