MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow FUSABOND™ N216 Anhydride-Modified Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene

Material Notes: Product Description: FUSABOND™ N216 is an anhydride modified ethylene elastomer.
Composition:
  • High% by weight maleic anhydride
  • Graft levels are defined as:
  • Low <0.2%; Medium 0.2-0.5%; High 0.5-1.0%; Ultra high >1.0%
Applications:
  • Impact modifier for polyamide blends with high MAH grafting level
  • Compatibilizer for flame retardant fillers in non-halogen flame retardant polyolefin-based wire and cable compounds
  • Compatibilizer or adhesion promoter between polyolefins and metals, polyamide, cellulose, and glass fibers.
Availability: Africa & Middle East; Asia Pacific; Europe: Latin America; North America

Additive: Flame Retardant; Impact Modifier

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.875 g/ccISO 1183
 0.877 g/ccASTM D792
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 1.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 108 °FFreezing point
 145 °F
Vicat Softening Point 104 °FASTM D1525
 104 °FISO 306
Glass Transition Temp, Tg -65.2 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF539 / 311232

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.