MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/ccTypical Carbon Steel
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 386 MPa
 71.0 MPa
@Temperature 649 °C
 105 MPa
@Temperature 538 °C
 143 MPa
@Temperature 538 °C
Tensile Strength, Yield 324 MPa
 55.8 MPa
@Temperature 649 °C
Elongation at Break 34 %
Modulus of Elasticity 201 GPa
 88.3 GPa
@Temperature 649 °C
 183 GPa
@Temperature 316 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air >= 1250 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel ASTM A 463 / SAE J1392 040 AHK, Grade 40 Aluminized Carbon Steel, Structural Steel (SS)
AK Steel Cold Rolled Carbon Steel, Commercial Steel (CS Type B), Standard Grade
AK Steel Hot Rolled Carbon Steel, Commercial Steel (CS Type B), Standard Grade
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
AK Steel Aluminized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade

NAKS079 / 14682

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.