MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals SURPASS® RMs341-UG sHDPE Rotational Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Rotational Molding Grade

Material Notes:

Octene Copolymer

Features:

  • Exceptional low temperature impact properties
  • Broad processing window
  • Low viscosity for exceptional processability, shorter cycle times, and energy saving
  • Superior whiteness for improved part appearance
  • Easy mold release
  • NSF listed for Standards #24, 51, 61
  • UL94 HB

Additives:

  • Processing antioxidant
  • UV stabilizer (estimated UV resistance >UV18)

Applications:

  • OEM custom and proprietary components
  • Recreational and leisure equipment
  • Containers, septic tanks and large fish boxes
  • Large tanks

United States: SURPASS RMs341-U(UG) resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may contact food only at temperatures of 212°F and below (21 CFR 176.170(c) Table 2, conditions of use B–H)

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.941 g/ccASTM D 792
ESCR 100% Igepal® >= 1000 hour
@Temperature 50.0 °C
F50; Condition A & B, 100% IGEPAL; ASTM D 1693
Melt Index of Compound 0.050 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.2 MPa
@Thickness 1.91 mm
Type IV specimen, 2" (50.8 mm) per minute test speed; ASTM D 638
Elongation at Yield 12 %
@Thickness 1.91 mm
Type IV specimen, 2" (50.8 mm) per minute test speed; ASTM D 638
Flexural Modulus 827 MPa
@Strain 1 %
ASTM D790
Impact Test 95.0 J
@Thickness 3.17 mm,
Temperature -40.0 °C
ARM Low Temperature Impact; ARM Method
 230 J
@Thickness 6.35 mm,
Temperature -40.0 °C
ARM Low Temperature Impact; ARM Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 126 °C(DSC)
Heat Distortion Temperature 43.0 °C
@Pressure 1.82 MPa
ASTM D648
 62.0 °C
@Pressure 0.455 MPa
ASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals SURPASS® RMs341-U sHDPE Rotational Molding Resin
ICO Polymers ICORENE™ 150-1501 HDPE Rotational Molding Resin
NOVA Chemicals SURPASS® RMs245-U sHDPE Rotational Molding Resin
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene
ICO Polymers ICORENE™ 150-1049 HDPE Rotational Molding Resin

PNOVB149 / 194757

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.