MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemglaze® V175 Polyurethane Coating  (discontinued **)
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where maximum performance properties are needed. These coatings provide the highest possible combinations of abrasion resistance, wear properties and flexibility. Use Chemglaze V-Line coatings as protective coatings for vinyl, Mylar®, ABS, FRP, and Noryl®.

Excellent wear is characteristic of all Chemglaze products. In laboratory evaluations 7.6 to 38.1 µm (0.3 to 1.5 mils) of Chemglaze V-Line polyurethane coatings provide better scuff and wear resistance than 50.8 - 76.2 µm (2 to 3 mils) of conventional scuff coats.

Flatting Concentrate

Socomore acquired the Aeroglaze® and Chemglaze® product lines from Lord in September 2016. This specific grade is discontinued and not a part of the Socomore product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccASTM D1475
Solids Content 20 %by weight; ASTM D2369 Modified
 20.5 %by volume; ASTM D2369 Modified
Volatile Organic Compounds (VOC) Content 732 g/lASTM D3960
Brookfield Viscosity 400 cPASTM D2196, LVT, Spindle #2 @ 30rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 32.0 °CASTM D3278, Seta Flash, Closed Cup
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 4.00 min
@Temperature 149 - 191 °C
 2.00 - 5.00 min
@Temperature 121 - 149 °C
 10.0 - 30.0 min
@Temperature 93.0 - 121 °C
 
Descriptive Properties
Theoretical Coverage (ft²/gallon/mil)328

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-7140 Polyurethane Foam
Sawbones Solid Rigid Polyurethane Foam 15 pcf Density
Socomore Chemglaze® V300 Polyurethane Coating
Socomore Chemglaze® V209 Polyurethane Coating
Socomore Aeroglaze® Z3480 High Solids Aromatic Polyurethane Coating

PLORD137 / 86145

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.