  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ravago Manufacturing Americas Hylon® N1200HL BK Nylon 6/6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes:
  • Available in North America
  • Additive: Heat Stabilizer and Lubricant
  • Features: Lubricated and Heat Stabilized
  • Auto Specifications: DELPHI QMPL-1257 Color: Black
  • Form: Pellets

Information provided by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D792
Density 1.14 g/ccISO 1183
Water Absorption 0.90 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.016 - 0.020 in/inASTM D955 and ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D785
Tensile Strength at Break 11000 psiASTM D638
 11000 psiISO 527-2
Elongation at Break 15 %ASTM D638
Flexural Strength 14000 psiASTM D790
 14100 psiISO 178
Flexural Modulus 410000 psiASTM D790
 410000 psiISO 178
Izod Impact, Notched 0.900 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 23.0 ft-lb/in²ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 460 °FUnannealed; ASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3Z HP UV BK23220 PA66 (Dry)
Envalior Stanyl® TW341 PA46, Dry, Heat Stabilized
Celanese Zytel® ST801AHS NC010 PA66-HI
Celanese Zytel® ST801 NC010A PA66-HI
Celanese Zytel® MT409AHS BK010 PA66-I

PENTA149a / 142979

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.