MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Silastic® LSR 9390-40 PARTS A&B  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes:

Former Dow/ Dow Corning brand.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
@Temperature 25.0 °C
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
Tensile Strength, Ultimate 754.21 psi
Elongation at Break 510 %
Tear Strength 11.0 pli
Compression Set 15 %
 
Processing PropertiesOriginal ValueComments
Pot Life 4320 min
Shelf Life 15.0 Month
 
Descriptive Properties
Coloroff-white
Mix Ratio (X:1)100Base to Catalyst ETN

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials Silopren™ LIM 6030 Liquid Silicone Rubber - Fast Cure / High Tear
Elkem (Bluestar Silicones) SILBIONE® LSR 4310 Liquid Silicone Rubber
Momentive Performance Materials RTV31 Silicone Rubber Compound for High Temperature, Red
Dow Silastic® 9280/70E KIT PARTS A&B
Dow Silastic® 3496 MOULD MAKING BASE & 96 CURING AGENT

PDOWCO547 / 106248

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.