MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel (Extended Electro-Magnetic Data)
Categories: Metal; Electronic/Magnetic Alloy

Material Notes: Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produced commercially by AK Steel, these magnetic materials exhibit their superior magnetic properties in the rolling direction. This directionality occurs because the steels are specially processed to create a very high proportion of grains within the steel which have similarly oriented atomic crystalline structures relative to the rolling direction.

In iron-silicon alloys, this atomic structure is cubic and the crystals are most easily magnetized in a direction parallel to the cube edges. By a combination of precise steel composition, rigidly controlled cold rolling and annealing procedures, the crystals of these oriented electrical steels are aligned with their cube edges nearly parallel to the direction in which the steel is rolled. Consequently, they provide superior permeability and lower core loss when magnetized in this direction.

AK Steel’s CARLITE grain Oriented Electrical Steels (GOES) products are supplied with CARLITE 3 insulative coating, an inorganic coating equivalent to ASTM A976 C-5. CARLITE 3 insulation is ideal for materials that will be used in the form of sheared laminations for power transformers and other apparatus with high volts per turn. In addition to supplying all the benefits of C-5 insulation, CARLITE 3 provides other important advantages which include:

  • Potential for reduced transformer building factor from added resistance to elastic strain damage
  • Potential for reduction of magnetostriction related transformer noise
  • High stacking factor
  • Easy assembly due to smoothness of coating (low coefficient of friction)

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.65 g/cc
Thickness 12.0 milNominal
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 167
Hardness, Rockwell B 81
Tensile Strength, Ultimate 51000 psiIn rolling direction
Tensile Strength, Yield 48000 psiIn rolling direction
Elongation at Break 9.0 %in 2"
Modulus of Elasticity 122 GPaIn rolling direction
 143 GPaat 20° to rolling direction
 200 GPaat 55° to rolling direction
 236 GPaat 90° to rolling direction
 258 GPaat 45° to rolling direction
 
Electrical PropertiesOriginal ValueComments
Exciting Power (RMS) 0.00398 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.00418 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.00496 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.00521 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.0135 RMS VA/lb
@Magnetic Field 0.200 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0138 RMS VA/lb
@Magnetic Field 0.200 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0171 RMS VA/lb
@Magnetic Field 0.200 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0174 RMS VA/lb
@Magnetic Field 0.200 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.0274 RMS VA/lb
@Magnetic Field 0.300 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0275 RMS VA/lb
@Magnetic Field 0.300 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0347 RMS VA/lb
@Magnetic Field 0.300 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0348 RMS VA/lb
@Magnetic Field 0.300 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.0447 RMS VA/lb
@Magnetic Field 0.400 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0448 RMS VA/lb
@Magnetic Field 0.400 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0567 RMS VA/lb
@Magnetic Field 0.400 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.0569 RMS VA/lb
@Magnetic Field 0.400 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0650 RMS VA/lb
@Magnetic Field 0.500 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0652 RMS VA/lb
@Magnetic Field 0.500 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0827 RMS VA/lb
@Magnetic Field 0.500 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.0831 RMS VA/lb
@Magnetic Field 0.500 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0882 RMS VA/lb
@Magnetic Field 0.600 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0887 RMS VA/lb
@Magnetic Field 0.600 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.112 RMS VA/lb
@Magnetic Field 0.600 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.113 RMS VA/lb
@Magnetic Field 0.600 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.114 RMS VA/lb
@Magnetic Field 0.700 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.115 RMS VA/lb
@Magnetic Field 0.700 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.144 RMS VA/lb
@Magnetic Field 0.800 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.145 RMS VA/lb
@Magnetic Field 0.800 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.147 RMS VA/lb
@Magnetic Field 0.700 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.147 RMS VA/lb
@Magnetic Field 0.700 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.177 RMS VA/lb
@Magnetic Field 0.900 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.178 RMS VA/lb
@Magnetic Field 0.900 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.185 RMS VA/lb
@Magnetic Field 0.800 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.186 RMS VA/lb
@Magnetic Field 0.800 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.215 RMS VA/lb
@Magnetic Field 1.00 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.215 RMS VA/lb
@Magnetic Field 1.00 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.228 RMS VA/lb
@Magnetic Field 0.900 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.229 RMS VA/lb
@Magnetic Field 0.900 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.258 RMS VA/lb
@Magnetic Field 1.10 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.259 RMS VA/lb
@Magnetic Field 1.10 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.276 RMS VA/lb
@Magnetic Field 1.00 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.277 RMS VA/lb
@Magnetic Field 1.00 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.309 RMS VA/lb
@Magnetic Field 1.20 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.309 RMS VA/lb
@Magnetic Field 1.20 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.331 RMS VA/lb
@Magnetic Field 1.10 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.332 RMS VA/lb
@Magnetic Field 1.10 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.371 RMS VA/lb
@Magnetic Field 1.30 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.372 RMS VA/lb
@Magnetic Field 1.30 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.396 RMS VA/lb
@Magnetic Field 1.20 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.396 RMS VA/lb
@Magnetic Field 1.20 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.452 RMS VA/lb
@Magnetic Field 1.40 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.456 RMS VA/lb
@Magnetic Field 1.40 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.474 RMS VA/lb
@Magnetic Field 1.30 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.476 RMS VA/lb
@Magnetic Field 1.30 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.572 RMS VA/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.575 RMS VA/lb
@Magnetic Field 1.40 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.580 RMS AT/cm
@Magnetic Field 1.40 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.582 RMS VA/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.722 RMS VA/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.733 RMS VA/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.783 RMS VA/lb
@Magnetic Field 1.60 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.788 RMS VA/lb
@Magnetic Field 1.60 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.975 RMS VA/lb
@Magnetic Field 1.60 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.980 RMS VA/lb
@Magnetic Field 1.60 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 1.34 RMS VA/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 1.45 RMS VA/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 1.65 RMS VA/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 1.78 RMS VA/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 3.76 RMS VA/lb
@Magnetic Field 1.80 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 4.11 RMS VA/lb
@Magnetic Field 1.80 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 4.57 RMS VA/lb
@Magnetic Field 1.80 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 4.99 RMS VA/lb
@Magnetic Field 1.80 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 13.8 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 14.7 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 16.8 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 18.0 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
Electrical Resistivity 0.0000510 ohm-cm
 
Magnetic PropertiesOriginal ValueComments
Core Loss 0.00195 W/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.00195 W/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.00259 W/lb
@Magnetic Field 0.100 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.00260 W/lb
@Magnetic Field 0.100 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.00750 W/lb
@Magnetic Field 0.200 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.00757 W/lb
@Magnetic Field 0.200 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0100 W/lb
@Magnetic Field 0.200 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0101 W/lb
@Magnetic Field 0.200 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.0164 W/lb
@Magnetic Field 0.300 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0165 W/lb
@Magnetic Field 0.300 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0219 W/lb
@Magnetic Field 0.300 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0220 W/lb
@Magnetic Field 0.300 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.0285 W/lb
@Magnetic Field 0.400 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0286 W/lb
@Magnetic Field 0.400 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0381 W/lb
@Magnetic Field 0.400 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.0381 W/lb
@Magnetic Field 0.400 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0437 W/lb
@Magnetic Field 0.500 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0437 W/lb
@Magnetic Field 0.500 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0580 W/lb
@Magnetic Field 0.500 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.0582 W/lb
@Magnetic Field 0.500 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0617 W/lb
@Magnetic Field 0.600 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0620 W/lb
@Magnetic Field 0.600 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0819 W/lb
@Magnetic Field 0.600 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.0823 W/lb
@Magnetic Field 0.600 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.0828 W/lb
@Magnetic Field 0.700 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.0833 W/lb
@Magnetic Field 0.700 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.107 W/lb
@Magnetic Field 0.800 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.108 W/lb
@Magnetic Field 0.800 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.110 W/lb
@Magnetic Field 0.700 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.111 W/lb
@Magnetic Field 0.700 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.134 W/lb
@Magnetic Field 0.900 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.136 W/lb
@Magnetic Field 0.900 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.142 W/lb
@Magnetic Field 0.800 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.143 W/lb
@Magnetic Field 0.800 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.165 W/lb
@Magnetic Field 1.00 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.166 W/lb
@Magnetic Field 1.00 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.178 W/lb
@Magnetic Field 0.900 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.180 W/lb
@Magnetic Field 0.900 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.199 W/lb
@Magnetic Field 1.10 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.201 W/lb
@Magnetic Field 1.10 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.218 W/lb
@Magnetic Field 1.00 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.220 W/lb
@Magnetic Field 1.00 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.238 W/lb
@Magnetic Field 1.20 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.240 W/lb
@Magnetic Field 1.20 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.263 W/lb
@Magnetic Field 1.10 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.266 W/lb
@Magnetic Field 1.10 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.281 W/lb
@Magnetic Field 1.30 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.283 W/lb
@Magnetic Field 1.30 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.314 W/lb
@Magnetic Field 1.20 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.317 W/lb
@Magnetic Field 1.20 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.330 W/lb
@Magnetic Field 1.40 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.332 W/lb
@Magnetic Field 1.40 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.371 W/lb
@Magnetic Field 1.30 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.374 W/lb
@Magnetic Field 1.30 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.390 W/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.390 W/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.390 W/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
Typical
 0.435 W/lb
@Magnetic Field 1.40 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.438 W/lb
@Magnetic Field 1.40 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 <= 0.440 W/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
 0.462 W/lb
@Magnetic Field 1.60 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.463 W/lb
@Magnetic Field 1.60 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.513 W/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.513 W/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.513 W/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
Typical
 0.563 W/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.566 W/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.566 W/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
Typical
 <= 0.580 W/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
 0.605 W/lb
@Magnetic Field 1.60 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 0.606 W/lb
@Magnetic Field 1.60 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 <= 0.630 W/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
 0.717 W/lb
@Magnetic Field 1.80 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.719 W/lb
@Magnetic Field 1.80 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.733 W/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.735 W/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
Typical
 0.736 W/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 <= 0.830 W/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
 0.895 W/lb
@Magnetic Field 1.90 T,
Frequency 50 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.898 W/lb
@Magnetic Field 1.90 T,
Frequency 50 Hz
Sheet, 0.012"; ASTM A804
 0.925 W/lb
@Magnetic Field 1.80 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 0.930 W/lb
@Magnetic Field 1.80 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 1.15 W/lb
@Magnetic Field 1.90 T,
Frequency 60 Hz
Sheet, 0.012"; ASTM A804
 1.15 W/lb
@Magnetic Field 1.90 T,
Frequency 60 Hz
Epstein Specimen, 0.012"; ASTM A343
 
Descriptive Properties
Magnetostriction 10^8-125At 60Hz, 1.7T (Thickness 0.012")
 -94At 60Hz, 1.5T (Thickness 0.012")
Minimum Lamination Factor (%)95.5
Minimum Peak Permeability at 10 Oe1780
Typical Lamination Factor (%)97.2
Typical Peak Permeability at 10 Oe1834

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel
AK Steel DI-MAX® M-36 Nonoriented Electrical Steel
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel (Extended Electro-Magnetic Data)
AK Steel DI-MAX® M-19 Nonoriented Electrical Steel

NAKS152a / 171255

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.