MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hanwha Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural, thin wall applications.

Commercially available only to European based customers.

Information provided by Azdel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccLaminate; ISO 2577
 1.22 g/ccMolded plaque; ISO 2577
Filler Content 40 %AZDEL Test
Thickness 3900 micronsAZDEL Test
Linear Mold Shrinkage 0.0025 cm/cm320 x 320 mm flat plaque; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527/4
Elongation at Break 2.5 %ISO 527/4
Tensile Modulus 5.50 GPaISO 527/4
Flexural Strength 150 MPaISO 178
Flexural Modulus 5.60 GPaISO 178
Charpy Impact, Notched 8.50 J/cm²ISO 179/2fn
Impact 5500
@Thickness 4.00 mm
N; Multi-axial at max. force; ISO 6603-2
Impact Test 17.0 J
@Thickness 4.00 mm
Multi-axial, at max. force; ISO 6603-2
 45.0 J
@Thickness 4.00 mm
Multi-axial, total energy; ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 29.0 µm/m-°C
@Temperature 0.000 - 120 °C
100 x 15 x 3 mm sample; AZDEL Test
 44.0 µm/m-°C
@Temperature -30.0 - 0.000 °C
100 x 15 x 3 mm sample; AZDEL Test
Melting Point 115 °CRecrystallizing temperature; ISO 3146
 155 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 160 °CISO 75/2a
 
Processing PropertiesOriginal ValueComments
Processing Temperature 205 - 220 °CSurface temperature
Mold Temperature 30.0 - 90.0 °C
Back Pressure 15.0 - 25.0 MPaDepending on wall thickness and part complexity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexTow® 1900/AS Chopped Carbon Fiber
Hanwha Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix

PZZGEAZ76 / 40625

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.