MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Pro-fax™ SC204 Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Description: Pro-fax™ SC204 polypropylene copolymer resin is designed for thermoforming and sheet extrusion applications. It is nucleated and features antistatic properties. Pro-fax™ SC204 resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients in Pro-fax™ SC204 resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Sheet, containers, thermoformed containers

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccASTM D792
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4700 psiASTM D 638
Elongation at Yield 7.0 %ASTM D 638
Flexural Modulus, 1% Secant 230000 psi0.05 in/min; ASTM D790
Izod Impact, Notched 2.00 ft-lb/in73°F; ASTM D256
Impact 14ft-lbs, Drop Weight Impact Strength, 4°C; Basell Test Method
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 244 °FUnannealed; ASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax™ RP320N Polypropylene Copolymer
LyondellBasell Pro-fax™ SC973 Polypropylene Copolymer
LyondellBasell Pro-fax™ SR257M Polypropylene Copolymer
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer
LyondellBasell Pro-fax™ PH835 Polypropylene Homopolymer

PMO879 / 53868

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.