MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EOS MS1 Maraging Steel Sintered on EOSINT M 270
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Maraging Steel

Material Notes: Steel powder processed by DMSL. This steel has very good mechanical properties, and is easily heat-treatable using a simple thermal age-hardening process to obtain excellent hardness and strength. This material is ideal for many tooling applications (DirectTool) such as tools for injection molding, die casting of light metal alloys, punching, extrusion etc., and also for high performance industrial and engineering parts, for example in aerospace and motor racing applications.

EOS®, EOSINT®, and DMLS® are registered trademarks of EOS GmbH. Information provided by Axis Prototyping.

Key Words: US classification 18% Ni Maraging 300, European 1.2709 and German X3NiCoMoTi 18-9-5
Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. Innovative leaders in producing high quality Rapid Prototyping and Rapid Manufacturing solutions using all major 3D printing systems including Stereolithography technology. Free online quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.0 - 8.1 g/cc
Porosity 0.0 %with standard processing parameters
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 33 - 37as built
 50 - 54after age hardening
Tensile Strength, Ultimate 1000 - 1200 MPaas built
 1670 - 2230 MPaafter age hardening
Tensile Strength, Yield 900 - 1100 MPa
@Strain 0.2 %
as built
 1800 - 2000 MPa
@Strain 0.2 %
after age hardening
Elongation at Break 1 - 3 %after age hardening
 5 - 11 %as built
Modulus of Elasticity 160 - 200 GPa
Charpy Impact 7.00 - 15.0 JNotched; after age hardening
 35.0 - 55.0 JNotched; as built
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.430 - 0.470 J/g-°Cas built
 0.430 - 0.470 J/g-°Cafter age hardening
Thermal Conductivity 14.2 - 15.8 W/m-Kas built
 19.0 - 21.0 W/m-Kafter age hardening
Maximum Service Temperature, Air 400 °C
Shrinkage 0.08 %
@Temperature 490 °C,
Time 21600 sec
age hardening
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.05 - 0.15 %
Carbon, C <= 0.03 %
Chromium, Cr <= 0.5 %
Cobalt, Co 8.5 - 9.5 %
Iron, Fe 64.6 - 69.35 %as balance
Manganese, Mn <= 0.1 %
Molybdenum, Mo 4.5 - 5.2 %
Nickel, Ni 17 - 19 %
Phosphorus, P <= 0.01 %
Silicon, Si <= 0.1 %
Sulfur, S <= 0.01 %
Titanium, Ti 0.6 - 0.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EOS PH1 Precipitation Hardening Stainless Steel Sintered on EOSINT M 270
AISI Type H13 Hot Work Tool Steel
AISI Grade 18Ni (300) Maraging Steel solution annealed at 815°C (1500°F) for 1 hour, air cooled, aged at 480°C (900°F) for 3 hours
Sandvik Osprey 1.2709 Tool Steel Powder
AISI Grade 18Ni (300) Maraging Steel nominal annealed properties

NEOS990 / 138559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.