MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HD 6207FL High Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HExxonMobil™ HD 6207FL is a homopolymer HDPE film grade designed to improve stiffness and barrier in coextrusion or in PE blends. When blended with LLDPE or metallocene LLDPE, ExxonMobil™ HD 6207FL improves their processability

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
  • Bread Bags
  • Collation Shrink
  • Food packaging
  • Form Fill and Seal Packaging
  • Freezer Film
  • General Packaging
  • Industrial Packaging
  • Label Film
  • Lamination Film
  • Multilayer Packaging Film
  • Overwrap Film
  • Packaging Films
  • Shoppers
  • Shrink Film
  • Stand Up Pouches

Information provided by ExxonMobil

Key Words: HDPE HTA 108
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.961 g/cc0.0347 lb/in³ASTM D4883
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 46.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
46.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 510 %510 %500 mm/min; ASTM D882
Film Elongation at Break, TD 2.00 %2.00 %500 mm/min; ASTM D882
Elmendorf Tear Strength MD 10 g10 gASTM D1922
Elmendorf Tear Strength TD 200 g200 gASTM D1922
Dart Drop Test <= 30.0 g<= 0.0662 lbASTM D1709A
Film Tensile Strength at Break, MD 60.0 MPa8700 psiASTM D882
Film Tensile Strength at Break, TD 31.0 MPa4500 psi500 mm/min; ASTM D882
1% Secant Modulus, MD 1170 MPa170000 psiASTM D882
1% Secant Modulus, TD 1720 MPa250000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 129 °C264 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin
Borealis Borstar® FB2230 LLDPE for Film
ExxonMobil HD 56200 High Density Polyethylene Resin
ExxonMobil LD 07523.AC Low Density Polyethylene Resin
ExxonMobil LD 07523.BW Low Density Polyethylene Resin

PEX99325 / 175561

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.