MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Solimide® TA-301-DODI Polyimide Foam
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Description: SOLIMIDE® foams offer a unique combination of properties suited for demanding industrial environments. Because the foams retain their flexibility at cryogenic temperatures, they are utilized as expansion joints for cryogenic tanks, pipelines and wind tunnels. Very low outgassing makes SOLIMIDE® foams the choice for use in sensitive electronic, medical and analytical instruments. These products can be used at temperatures that would degrade other foams, allowing for use as insulation in ovens and other high temperature processes. SOLIMIDE® foams are used in a variety of applications from transportation to plant maintenance. They are environmentally "green," chemical and fire resistant, lightweight, durable, easy to install, and can be customized for any industrial situation. Meets U.S. Mil Spec DOD-I-24688.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.440 lb/ft³ASTM D3574A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 0.0600 MPaASTM D3574E
Compressive Strength 0.00900 MPa50% Compression Force Deflection; ASTM D3574B
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0420 W/m-KASTM C518
Flammability Test 3.0Specific Optical Density of Smoke, Non-Flaming; ASTM E662
 5.0Specific Optical Density of Smoke, Flaming; ASTM E662
Flame Spread Index >= 5.0Radiant Panel; ASTM E162
 
Descriptive Properties
Acoustical Absorption Coefficient (1000Hz)0.98 sabins/m225 mm, ASTM C423 and E795, Type A Mounting
 1.02 sabins/m250 mm, ASTM C423 and E795, Type A Mounting
Acoustical Absorption Coefficient (125 Hz)0.11 sabins/m225 mm, ASTM C423 and E795, Type A Mounting
 0.32 sabins/m250 mm, ASTM C423 and E795, Type A Mounting
Acoustical Absorption Coefficient (2000 Hz)0.87 sabins/m250 mm, ASTM C423 and E795, Type A Mounting
 0.97sabins/m225 mm, ASTM C423 and E795, Type A Mounting
Acoustical Absorption Coefficient (250 Hz)0.21 sabins/m225 mm, ASTM C423 and E795, Type A Mounting
 0.53 sabins/m250 mm, ASTM C423 and E795, Type A Mounting
Acoustical Absorption Coefficient (4000 Hz)0.81 sabins/m225 mm, ASTM C423 and E795, Type A Mounting
 0.90 sabins/m250 mm, ASTM C423 and E795, Type A Mounting
Acoustical Absorption Coefficient (500 Hz)0.56 sabins/m225 mm, ASTM C423 and E795, Type A Mounting
 0.94 sabins/m250 mm, ASTM C423 and E795, Type A Mounting
Noise Reduction Coefficient0.725 mm, ASTM C423 and E795, Type A Mounting
 0.8550 mm, ASTM C423 and E795, Type A Mounting
Toxic Gas Generation
  • 180 ppm CO
  • Max 1 ppm HCN
  • Max 1 ppm HF
  • Max 10 ppm HCl
  • Max 1 ppm NOx
  • Max 1 ppm SO2
Boeing BSS 7239, flaming mode

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Solimide® TA-301 Polyimide Foam
Evonik Solimide® AC-530-AIMS Polyimide Foam
Avient Melos® FM 976 Ethylene-Propylene Diene Elastomer (EPDM) Compound
Evonik Solimide® AC-530-MMS-BMS Polyimide Foam
Evonik Solimide® HT-340 Polyimide Foam

PHUK110 / 47244

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.