MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tipco Tipcolene® FPC 10 - 10% Calcium Carbonate Reinforced Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: 10% Calcium Carbonate Filled PP Homopolymer

Applications: General Purpose

Processing: Injection Molding

Information provided by the Manufacturer, Tipco Industries Ltd., India.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccASTM D792
Linear Mold Shrinkage 0.017 cm/cmASTM D955
Melt Flow 10 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 31.0 MPaASTM D638
Elongation at Break >= 50 %ASTM D638
Flexural Yield Strength 33.0 MPaASTM D790
Flexural Modulus 1.765 GPaASTM D790
Izod Impact, Notched (ISO) 4.50 kJ/m²ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Buckeye Polymers BP RPP 0511C Polypropylene, 5% Mineral Filled
Dow INSPIRE™ TF1300 Polypropylene
Buckeye Polymers BP RPP 1012 C Polypropylene, 10% Mineral Filled
Trinseo INSPIRE™ TF0808S(U) Polypropylene
Multibase Multi-Pro® 1012 C BLK Medium Impact Mineral Filled Polypropylene

PTIP010 / 70246

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.