MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems DuraForm® GF Glass Filled Nylon
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: For use with all selective laser sintering (SLS®) systems.

    Applications
  • Housings and enclosures
  • Consumer sporting goods
  • Appropriate for low- to mid-volume rapid manufacturing
  • Parts requiring machining or joining with adhesives
  • Complex production and prototype plastic parts
  • Form, fit, or functional prototypes
  • Parts requiring stiffness
  • Thermally stressed parts

All information provided by 3D Systems.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/ccASTM D792
Water Absorption 0.22 %
@Time 86400 sec
0.22 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7777ASTM D2240
Tensile Strength, Ultimate 26.0 MPa3770 psiASTM D638
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Break 1.4 %1.4 %ASTM D638
Tensile Modulus 4.068 GPa590.0 ksiASTM D638
Flexural Strength 37.0 MPa5370 psiUltimate; ASTM D790
Flexural Modulus 3.106 GPa450.5 ksiASTM D790
Izod Impact, Notched 0.410 J/cm
@Temperature 23.0 °C
0.768 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched 1.23 J/cm
@Temperature 23.0 °C
2.30 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Gardner Impact 4.50 J3.32 ft-lbASTM D5420
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.20e+11 ohm-cm3.20e+11 ohm-cmASTM D257
Surface Resistance 3.20e+11 ohm3.20e+11 ohmASTM D257
Dielectric Constant 6.27
@Frequency 1000 Hz
6.27
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 8.70 kV/mm221 kV/inASTM D149
Dissipation Factor 0.177
@Frequency 1000 Hz
0.177
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  62.3 µm/m-°C
@Temperature 0.000 - 50.0 °C
34.6 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831
 124.6 µm/m-°C
@Temperature 85.0 - 145 °C
69.22 µin/in-°F
@Temperature 185 - 293 °F
ASTM E831
Specific Heat Capacity 1.09 J/g-°C0.261 BTU/lb-°FASTM E1269
Thermal Conductivity 0.470 W/m-K3.26 BTU-in/hr-ft²-°FASTM E1225
Deflection Temperature at 0.46 MPa (66 psi) 179 °C354 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 134 °C273 °FASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems DuraForm® PA Nylon for SLS® Systems
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Polyetheretherketone, Unreinforced
3D Systems DuraForm® AF Nylon for SLS® Systems

PAPPR116 / 83495

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.