MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Alpase K100™ Aluminum Plate  (discontinued **)
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: K100™ features and benefits include: Dimensional stability, excellent machinability, fully weldable, anodizable, stress relieved, equiaxial grain structure, custom sizes available.

Applications:Machinery, fixtures, templates, packaging equipment (frames, bracing, sides), medical equipment (X-ray machines, tables), gauges (close tolerance arms & slides), vacuum chucks (milling machines and lathes), indexing tables, printing and robotic equipment.

Sizes: Thickness 0.25 - 30 inches; Width 12 - 120.5 inches; Length 24 - 325 inches. Data provided by Alpase.

Key Words: Aluminium
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 55 - 65
Tensile Strength, Ultimate 165 MPaTypical
Tensile Strength, Yield 83.0 MPaTypical
Elongation at Break 2.0 - 3.0 %Typical
Modulus of Elasticity 71.7 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000440 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 147 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 93 %as balance
Copper, Cu 1.0 - 1.4 %
Iron, Fe 0.50 - 1.0 %
Magnesium, Mg 0.90 - 1.5 %
Manganese, Mn 0.30 - 0.50 %
Silicon, Si 0.050 - 1.0 %
Zinc, Zn 2.5 - 4.0 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alpase K100-S™ Aluminum Plate
Alcoa MIC-6 Aluminum Mold Alloy
515.0 Aluminum Composition Spec
Aluminum 6061-T6; 6061-T651
PCP-Canada ALCA 5® 5083 Cast Aluminum Mold Plate

NALPASE1 / 14950

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.