System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Ravago Manufacturing Americas Hylac® HF96 ABS
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Molded
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.
Information provided by Ravago.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.03
g/cc
ASTM D792
Linear Mold Shrinkage
0.0030
-
0.0070
cm/cm
0.125 in; ASTM D955
Melt Flow
3.0
g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
8.5
g/10 min
@Load 3.80 kg,
Temperature 230 °C
Cond I; ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
102
ASTM D785
Tensile Strength, Yield
6200
psi
ASTM D638
Elongation at Break
30 %
ASTM D638
Tensile Modulus
360000
psi
ASTM D638
Flexural Yield Strength
9200
psi
ASTM D790
Flexural Modulus
335000
psi
ASTM D790
Izod Impact, Notched
4.60
ft-lb/in
0.25 in; ASTM D256
5.50
ft-lb/in
73°F, 0.125 in; ASTM D256
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+15
ohm-cm
ASTM D257
Thermal Properties
Original Value
Comments
CTE, linear
64.0
µin/in-°F
@Temperature -40.0 - 176 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi)
203
°F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
188
°F
Unannealed; ASTM D648
Vicat Softening Point
210
°F
ASTM D1525
Flammability, UL94
HB
@Thickness 1.50 mm
Processing Properties
Original Value
Comments
Rear Barrel Temperature
355
-
390
°F
Middle Barrel Temperature
390
-
430
°F
Front Barrel Temperature
420
-
455
°F
Nozzle Temperature
410
-
445
°F
Melt Temperature
465
°F
Mold Temperature
120
-
140
°F
Moisture Content
<= 0.10 %
Injection Pressure
850
-
1000
psi
Back Pressure
70.0
-
140
psi
Shot Size
40 - 80 %
Screw Speed
50
-
90
rpm
Descriptive Properties
Holding Pressure
710 to 850 psi
Injection Rate
Slow-Moderate
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Albis Plastics ABS 01A HI01 Unreinforced
INEOS Styrolution Terluran® EGP-7 ABS
INEOS Styrolution Terluran® HI-10 ABS
Aclo Accucomp ABS ABS846HL High Flow Medium Impact Grade
Ineos ABS Lustran® 648
PENTA031 / 36040
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.