MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Entira® ASSD100 Ionomer Resin
Categories: Polymer; Thermoplastic; Ionomer

Material Notes: DuPont™ Entira™ AS SD100 is an extremely hygroscopic ionomer resin that is supplied as free flowing pellets.

Entira™ AS SD100 is used to lower the static decay time and surface resistivity of LDPE, LLDPE and other polymers. Entira™ AS SD100 can be precompounded or dry blended into polymers for extrusion, molding, or various other processing methods. Antistatic agent for polyethylene ( LDPE, LLDPE and EVA) and other polymers, in films, moldings and extruded forms.

Entira™ AS SD100 resin complies with the U.S. Food and Drug Administration Regulation 21 CFR 177.1330(a) -- Ionomeric resins, subject to the limitations and requirements therein. This Regulation describes polymers that may be in contact with non-alcoholic food, subject to the finished food contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (c) of the Regulation.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.985 g/ccASTM D792, ISO 1183
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 64.0 °CFreezing Point; ASTM D3418
 92.0 °CASTM D3418, ISO 3146
Vicat Softening Point 63.0 °CASTM D1525, ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 210 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer
Abatron TDS, AboThane 861019/8606-5 Acrylic/Polyurethane Enamel
Dow Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy

PDTA4951 / 170391

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.