MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AK Steel 201 Austenitic Stainless steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed condition but slightly magnetic when cold worked. Excellent toughness at low temperatures. Typical uses include appliances, restaurant equipment, cooking utensils, sinks, automotive trim, architectural applications such as windows and doors, railway cars, trailers and hose clamps.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.81 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 87Annealed
Hardness, Rockwell C 25Cold Worked 1/4 hard
 32Cold Worked 1/2 hard
 41Cold-Worked Full hard
Tensile Strength, Ultimate 758 MPaAnnealed
 862 MPaCold-Worked 1/4 hard
 1034 MPaCold-Worked 1/2 hard
 1276 MPaCold-Worked Full hard
Tensile Strength, Yield 379 MPa
@Strain 0.2 %
Annealed
 517 MPa
@Strain 0.2 %
Cold-Worked 1/4 hard
 758 MPa
@Strain 0.2 %
Cold-Worked 1/2 hard
 965 MPa
@Strain 0.2 %
Cold-Worked Full hard
Elongation at Break 8.0 %in 2 inches, Cold-Worked Full hard
 15 %in 2 inches, Cold-Worked 1/2 hard
 25 %in 2 inches, Cold-Worked 1/4 hard
 52 %in 2 inches, Annealed
Modulus of Elasticity 197 GPa
Izod Impact 163 JV-Notch (Annealed)
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000685 ohm-cm
Magnetic Permeability 1.02H = 200 Oersted, Annealed
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.7 µm/m-°C
@Temperature 0.000 - 100 °C
 20.3 µm/m-°C
@Temperature <=871 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.2 W/m-K
@Temperature 100 °C
 21.4 W/m-K
@Temperature 500 °C
Melting Point 1399 - 1454 °C
Solidus 1399 °C
Liquidus 1454 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 16 - 18 %
Iron, Fe 67.51 - 75 %As Remainder
Manganese, Mn 5.5 - 7.5 %
Nickel, Ni 3.5 - 5.5 %
Nitrogen, N <= 0.25 %
Phosphorus, P <= 0.060 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed
304 Stainless Steel
AK Steel 201LN Austenitic Stainless steel
AK Steel 301 Austenitic Stainless steel
202 Stainless Steel, Annealed Bar

NAKS105 / 14708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.