MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NAECO® NAECOMET® D582F Silver Graphite Contact Material
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Precious Metal; Silver Alloy

Material Notes: For electrical contacts; reduced sticking, low voltage DC

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.4 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 45 - 7345 (annealed) - 73 (worked)
Tensile Strength, Ultimate 172 MPaAnnealed
 255 MPaWorked
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000167 ohm-cm(103% IACS)
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 980 °C
Liquidus 980 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.25 %
Silver, Ag 99.75 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NAECO® NAECOMET® D58 Silver Graphite Contact Material
NAECO® NAECOMET® D581F Silver Graphite Contact Material
NAECO® NAECOMET® D158F Silver Graphite Contact Material
NAECO® NAECOMET® D1058 Silver Graphite Contact Material
NAECO® NAECOMET® D154X Post-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3

NCMV826 / 192406

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.