MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sirmax Dafnestill® AM Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: Medium impact polystyrene, easy flow, high stiffness.

Application: Injection Molding

Information provided by Sirmax®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Water Absorption <= 0.10 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 70ISO 2039-2
Tensile Strength, Yield 23.0 MPa50 mm/min; ISO 527-2
Elongation at Break 40 %50 mm/min; ISO 527-2
Flexural Strength 45.0 MPa2 mm/min; ISO 178
Flexural Modulus 2200 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²ISO 180/1A
Charpy Impact, Notched 6.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 7.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.50e+15 ohmIEC 60093
Comparative Tracking Index 375 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CISO 75/Af
Vicat Softening Point 85.0 °CB50; ISO 306
 94.0 °CA50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
Glow Wire Flammability Index 650 °C
@Thickness 1.50 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 220 °CISO 294
Mold Temperature 20.0 - 60.0 °CISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIRMX073 / 281176

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.