MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bakelite® PF 6510 Phenolic Molding Compound
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant.

Applications: Thermally and mechanically highly stressed parts in automotive field, water pump housing, cooling media resistant

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccISO 1183
Apparent Bulk Density 0.740 g/ccISO 60
Linear Mold Shrinkage 0.0020 cm/cmInjection Molding. Post Shrinkage = 0.05%.; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 100 MPaISO 527 - 1/2
Tensile Modulus 16000 MPaISO 527 - 1/2
 11.0 GPa
@Temperature 150 °C
as molded & with post cure; ISO 527 - 1/2
 20.0 GPa
@Temperature 23.0 °C
as molded & with post cure; ISO 527 - 1/2
Flexural Strength 210 MPaISO 178
Flexural Modulus 16000 MPaISO 178
Compressive Strength 260 MPaISO 604
Poissons Ratio 0.32no post cure
Charpy Impact Unnotched 15.5 kJ/m²ISO 179-1 eU
Charpy Impact, Notched 4.00 kJ/m²ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cm
Surface Resistance 1.00e+11 ohm
Dielectric Constant 5.5
@Frequency 100 Hz
Dielectric Strength 32.0 kV/mm
@Thickness 1.00 mm
IEC 60243-P1
Dissipation Factor 0.050
@Frequency 100 Hz
Comparative Tracking Index 200 VTest Liquid A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 11.0 µm/m-°Cno post cure
CTE, linear, Transverse to Flow 25.0 µm/m-°Cno post cure
Deflection Temperature at 8.0 MPa 175 °CISO 75-2
Flammability, UL94 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
@Temperature <=20.0 °C
50-60% RH
 
Descriptive Properties
Water absorption (mg)1224h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® PF 1110 Phenolic Molding Compound
Bakelite® PF 2717 Phenolic Molding Compound
Bakelite® PF 6501 Phenolic Formaldehyde Resin, Low Shrinkage
Bakelite® PF 7582 Phenolic Molding Compound
Menzolit Menzolit® BMC 1400 Unsaturated Polyester UP

PBAKE986 / 192348

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.