MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance.
  • Excellent flexural, impact, and tensile characteristics
  • Very high continuous working temp
  • Very high heat distortion temp
  • Exceptional chemical resistance
  • Superior dielectric at high temperatures and frequencies
  • Good radiation resistance
  • Outstanding wear and abrasion resistance
  • Low smoke and toxic gas emissions
  • Excellent hydrolysis resistance

Information Provided by Ensinger Inc.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.0477 lb/in³ASTM D792
Water Absorption 0.50 %at 24 hours; ASTM D570
Water Absorption at Saturation 0.50 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 99ASTM D785
Tensile Strength, Yield 16000 psiASTM D638
Elongation at Break 40 %ASTM D638
Elongation at Yield 4.9 %ASTM D638
Tensile Modulus 650000 psi1 % Sec; ASTM D638
Flexural Strength 26000 psiASTM D790
Flexural Modulus 600000 psiTangent; ASTM D790
Compressive Strength 17100 psiASTM D695
Shear Strength 7600 psiUltimate; ASTM D3846
Izod Impact, Notched 1.55 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.181200 in/min, 155 lbs Load; ASTM D1894-95
Limiting Pressure Velocity 170000 psi-ft/min1200 in/min
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.90e+16 ohm-cmASTM D257
Dielectric Strength 500 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 26.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 1.70 BTU-in/hr-ft²-°FASTM C177
Melting Point 633 °F
Maximum Service Temperature, Air 500 °FContinuous
Deflection Temperature at 1.8 MPa (264 psi) 320 °FASTM D648
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)
Ensinger Tecapeek® PVX Polyetheretherketone (PEEK)
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Afton Plastics 450G PEEK Polyetheretherketone

PENS24 / 35980

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.