Calprene H6174 is a 67/33 linear structure ethylene-butylene/styrene thermoplastic copolymer, polymerized in solution, with a high molecular weight and excellent ozone resistance. This product gives an excellent surface appearance to the injected or extruded compounds Applications: Technical Compounding: especially indicated for high quality surface appearance compounds transformed by injection or by extrusion Plastic modification This product is available in: CH 6174: porous crumbs CH6174S: porous crumbs dusted WITH amorphous silica CH 6174 P: powder form dusted WITH amorphous silica CH 6174 PH: powder form WITHOUT any dusting agent Information provided by Dynasol. |