MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Solaxis FDM Nylon 12 3D Printing Polymer, Conditioned
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: FDM Nylon 12™ is the first material in Stratasys’ family of nylon offerings, complementing the current portfolio of FDM® materials and enabling new applications requiring: repetitive snap fits, high fatigue resistance, strong chemical resistance and press (friction) fit inserts. FDM Nylon 12 is primarily used in aerospace, automotive and consumer goods industries to take on everything from tooling, jigs and fixtures to covers, panels and vibration resistant components. For use with Fortus 380mc™, 450mc™ and 900mc™ 3D Printers, FDM Nylon 12 offers unparalleled toughness and a simple, clean process – free of powders.

Information provided by Solaxis Ingenious Manufacturing

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 38.5 MPa
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 46.0 MPa
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Tensile Strength, Yield 28.0 MPa
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 32.0 MPa
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Elongation at Break 5.4 %
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 30 %
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Elongation at Yield 2.4 %
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
 2.7 %
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
Tensile Modulus 1.138 GPa
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 1.282 GPa
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Flexural Strength 61.0 MPaZX Axis, Method 1, 0.05 in./min; ASTM D790
 67.0 MPaXZ Axis, Method 1, 0.05 in./min; ASTM D790
Flexural Modulus 1.18 GPaZX Axis, Method 1, 0.05 in./min; ASTM D790
 1.275 GPaXZ Axis, Method 1, 0.05 in./min; ASTM D790
Flexural Strain at Break >= 10 %ZX Axis; ASTM D790
Compressive Yield Strength 51.0 MPaXZ Axis, Method 1, 0.05"/min; ASTM D695
 55.0 MPaZX Axis, Method 1, 0.05"/min; ASTM D695
Compressive Strength >= 6.00 MPaZX Axis, Method 1, 0.05"/min; ASTM D695
 >= 167 MPaXZ Axis, Method 1, 0.05"/min; ASTM D695
Compressive Modulus 1.069 GPaZX Axis, Method 1, 0.05"/min; ASTM D695
 5.033 GPaXZ Axis, Method 1, 0.05"/min; ASTM D695
Izod Impact, Notched 53.0 J/mZX Axis, Method A; ASTM D256
 135 J/mXZ Axis, Method A; ASTM D256
Izod Impact, Unnotched 200 J/mZX Axis, Method A; ASTM D256
 1656 J/mXZ Axis, Method A; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °Cunannealed; ASTM D648
 97.0 °Cannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °Cunannealed; ASTM D648
 82.0 °Cannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLXIS984 / 256141

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.