MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
95% Alumina, vitreous body
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Good Thermal Shock resistance, Tc value = 800-1100°C (1470-2010°F).

Key Words: aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.61 - 3.75 g/cc
Water Absorption 0.00 %24 hrs
Open Porosity <= 1.0 %Hermetic (helium mass spectrometer test on 0.254 mm (0.010 in) sections)
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 1720
Hardness, Mohs 9.0
Tensile Strength, Ultimate 170 - 240 MPa
Modulus of Elasticity 270 - 295 GPa
Flexural Strength 310 - 345 MPa
Charpy Impact, Notched 0.700 - 0.860 J/cm²
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 6.00e+8 ohm-cm
@Temperature 700 °C
 9.00e+14 ohm-cm
@Temperature 100 °C
 1.00e+16 ohm-cm
@Temperature 25.0 °C
Dielectric Strength 9.84 - 15.7 kV/mm(AC)
 0.790 - 1.18 kV/in
@Temperature 1000 °C
AC
 3.94 - 4.72 kV/in
@Temperature 500 °C
AC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.70 - 6.67 µm/m-°C
@Temperature 25.0 - 200 °C
 6.70 - 7.65 µm/m-°C
@Temperature 25.0 - 600 °C
 7.60 µm/m-°C
@Temperature 25.0 - 800 °C
 8.07 µm/m-°C
@Temperature 25.0 - 700 °C
 8.45 - 9.14 µm/m-°C
@Temperature 25.0 - 1000 °C
Specific Heat Capacity 0.437 - 0.442 J/g-°C
Thermal Conductivity 19.0 - 22.0 W/m-K
@Temperature 38.0 °C
 35.0 W/m-K
@Temperature 425 °C
 43.0 W/m-K
@Temperature 870 °C
Maximum Service Temperature, Air 1600 - 1700 °Cmaximum working temperature
 
Component Elements PropertiesOriginal ValueComments
Al2O3 95 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
85% Alumina, vitreous body
92% Alumina, opaque
96% Alumina, thick-film, as fired
99.5% Alumina, vitreous body
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3

BA2D / 138

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.