MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUPOL GP3202 PP+MF20%
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Description: Injection Molding, PP+MF10%, General Purpose, Good Weatherability

Application: Electrical, Electronic and Automotive Interior Parts

CAS: 9003-07-0 and 14807-96-6

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Maximum Moisture Content 0.010Injection Molding
Linear Mold Shrinkage, Flow 0.0090 - 0.013 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 300 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 45 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 450 kg(f)/cm²
@Thickness 6.40 mm
30mm/min; ASTM D790
Flexural Modulus 27000 kg(f)/cm²
@Thickness 6.40 mm
30mm/min; ASTM D790
Izod Impact, Notched >= 3.50 kg-cm/cm
@Thickness 6.40 mm,
Temperature -10.0 °C
ASTM D256
 >= 6.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
@Thickness 3.20 mm
Unannealed; ASTM D648
UL RTI, Electrical 65.0 °C
@Thickness >=1.50 mm
UL RTI, Mechanical with Impact 65.0 °C
@Thickness >=1.50 mm
UL RTI, Mechanical without Impact 65.0 °C
@Thickness >=1.50 mm
Flammability, UL94 HB
@Thickness >=1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 - 210 °CInjection Molding
Middle Barrel Temperature 200 - 230 °CInjection Molding
Front Barrel Temperature 200 - 230 °CInjection Molding
Nozzle Temperature 210 - 230 °CInjection Molding
Melt Temperature 200 - 230 °CInjection Molding
Mold Temperature 40.0 - 60.0 °CInjection Molding
Drying Temperature 70.0 - 80.0 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPaInjection Molding
Screw Speed 30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOL GP3200 PP+MF20%
IRPC Polimaxx Polene 1100NK Polypropylene Homopolymer
LG Chemical LUPOL HM3207 PP+MF20%, High Stiffness
Avient Maxxam® 6530-1001 Polypropylene (PP), Talc Filled
Avient Maxxam® 6529-1001 Polypropylene (PP), Talc Filled

PLAY469 / 148479

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.