MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Melinex® 581 Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: A super clear, one side C-Sub pretreated film for adhesion of hydrophilic coatings.

Approvals: UL Recognition - Product has been registered with Underwriters Laboratories

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 14500 psiASTM D882A
Film Elongation at Break, MD 170 %ASTM D882A
Film Elongation at Break, TD 120 %ASTM D882A
Coefficient of Friction, Dynamic 0.50A-B; ASTM D1894
Film Tensile Strength at Break, MD 28000 psiASTM D882A
Film Tensile Strength at Break, TD 35000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 2.5 %
@Temperature 190 °C,
Time 300 sec
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 190 °C,
Time 300 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 88 %
@Thickness 0.127 mm
TLT; ASTM D1003
 89 %
@Thickness 0.102 mm
TLT; ASTM D1003
 90 %
@Thickness 0.0635 mm
TLT; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 542 Polyester Film
DuPont Teijin Films Melinex® 617 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® 565 Polyester Film
DuPont Teijin Films Melinex® 561 Polyester Film
DuPont Teijin Films Melinex® 583 Polyester Film, 300 Gauge

PDTZ9166 / 139514

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.