MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
H.C. Starck Grade A Zirconium Diboride, ZrB2
Categories: Ceramic; Boride

Material Notes:
  • Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizing
  • Crucible material for non-ferrous metals
  • Ceramic shapes to be used in production of Al in Hall-Heroult cells
  • Hot pressed TiB, armor plates
  • Cutting tools and cermets, suitable for machining aluminum
  • Metal Matrix Composites
  • Antioxidant in carbon-bonded refractories
  • Burnable absorbers for neutrons

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 3.0 - 5.0 µmAverage Particle Size/Laser Diffraction D50
 <= 12 µm90% less than
 
Component Elements PropertiesOriginal ValueComments
Hafnium, Hf >= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
H.C. Starck Grade HD 20 Boron Carbide, B4C
H.C. Starck Grade UF 10 Silicon Carbide, SiC
Silicon Carbide, Alpha SiC
Zirconium Boride, ZrB2
3M Techical Ceramics Titanium Diboride

CHCSTA006 / 1184

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.