MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 2599 X 125099 Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - Carbon Fiber - EMI/RFI Shielding - Electrically Conductive
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Antistat/Conductive; Polycarbonate (PC)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D 792
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 11000 psiASTM D 638
Elongation at Break 1.6 %ASTM D 638
Tensile Modulus 1000 ksiASTM D 638
Flexural Strength 17800 psiASTM D 790
Flexural Modulus 1000 ksiASTM D 790
Izod Impact, Notched 3.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 5.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.0 ohm-cmASTM D 257
Surface Resistance <= 100 ohmESD STM11.11
Surface Resistivity per Square <= 1000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness 58 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 61 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 64 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 67 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 74 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 75 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 78 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 81 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 84 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 92 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 95 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 96 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 255 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 485 - 525 °F
Mold Temperature 110 - 140 °F
Drying Temperature 200 °F
@Time 14400 sec
Moisture Content 0.020 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI LATISHIELD 36/AR-05A-V0 Acrylonitrile Butadiene Styrene (ABS) Base E.M.I. Shielding Plastic (UL94 V-0)
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic
RTP Company EMI 2162 Polyetherimide (PEI); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1382  Polyphenylene Sulfide (PPS) Shielding - Nickel-Coated Carbon Fiber 15%

PQZUA18085 / 134678

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.